Hastelloy c276/ UNS N10276/ DIN 2.4819/ NAS NW276/ NW 0276 nickel alloy steel corrosion resistance wn/blind/slip on/ socket weld/thread flanges
Hastelloy C-276 alloy is Ni-Cr-Mo alloy steel, which has excellent corrosion resistance in oxidation-reduction environment.
1. Chemical Composition
| C |
≤0.01 |
| Si |
≤0.08 |
| Mn |
≤1.0 |
| P |
≤0.04 |
| S |
≤0.03 |
| Cr |
14.5-16.5 |
| Mo |
15.0-17.0 |
| Fe |
4.0-7.0 |
| Co |
≤2.5 |
| W |
3.0-4.5 |
| V |
≤0.35 |
2. Mechanical Properties
| YS(N/mm2) |
≥283 |
| TS(N/mm2) |
≥690 |
| EL(%) |
≥40 |
| HRB |
≤100 |
3. Physical Properties
| Density(g/cm3) |
8.9 |
| Specific Heat(J/kg.K) |
436 |
| Resistivity(μΩ.cm) |
130 |
| Thermal Conductivity(W/m.K) |
10.8 |
| Thermal diffusivity(m2/s) |
2.8×10-6 |
| Average thermal expansion coefficient(10-6/℃) |
20-100℃ |
12.2 |
| 20-200℃ |
12.5 |
| 20-300℃ |
12.9 |
| 20-400℃ |
13.2 |
| 20-500℃ |
13.6 |
| Longitudinal modulus of elasticity(Mpa) |
21.1×104 |
| Modulus of rigidity(Mpa) |
80.8×104 |
| Ferromagnetic |
No |
| Melting Point(℃) |
1325-1369 |